Skip to content
☎ +27 81 587 5010WhatsApp Find an ApplicatorSamples Data sheetsGallery
APPLICATION CONDITIONS · 4 min read · Last reviewed: November 2026

What Temperature, Humidity and Dew Point Conditions are Needed?

SHORT ANSWERGUIDE

Resin floors are sensitive to temperature, humidity and condensation while they cure. Keep the substrate and air within the MDS range, and keep the substrate at least 3 °C above the dew point during application and early cure.

Why conditions matter

Resins cure by chemical reaction, and that reaction depends on temperature. Too cold and the floor cures slowly or incompletely. Too hot and working time shortens sharply. High humidity and condensation can leave a greasy film on epoxies, known as amine blush, which spoils gloss and the bond of the next coat.

The dew point rule

The dew point is the temperature at which moisture in the air condenses onto a surface. If the slab is at or near it, a film of water forms that you may not see. The widely used safety margin is to keep the substrate at least 3 °C above the dew point.

Key checks

ParameterTypical requirementHow to measure
Substrate temperatureWithin the MDS range, often around 10 to 30 °CInfrared or contact thermometer
Air temperatureWithin the MDS rangeThermometer
Air relative humidityBelow the MDS limit, often around 80 to 85%Hygrometer
Dew point marginSubstrate at least 3 °C above dew pointDew point meter or calculator
Temperature trendStable or falling preferredLog readings through the day

Method overview

  1. Measure before mixing. Record substrate temperature, air temperature, humidity and dew point.
  2. Condition the space. Heat and dehumidify where needed, using indirect or electric heating.
  3. Store materials correctly. Keep components at the temperature the MDS recommends.
  4. Watch rising temperatures. A warming slab releases air through pores, causing pinholes. Applying as temperatures fall reduces this.
  5. Hold conditions through cure. Maintain the range until the MDS cure time has passed.
  6. Ventilate. Provide fresh air without creating draughts or dust.

Common failure modes

SymptomLikely causePrevention
Sticky or greasy surfaceAmine blush from cold or humid conditionsControl conditions; follow MDS recoat advice
Pinholes or bubblesOutgassing as slab temperature risesApply on falling temperatures; seal porous substrates
Slow or soft cureToo coldHeat the space and substrate
Lap marks, short working timeToo hotWork in cooler periods; smaller mixes
Water marks or dull patchesCondensationKeep 3 °C above dew point
Safety note: Do not use unvented gas or paraffin heaters during application or cure. They add moisture and carbon dioxide that can damage the floor surface, and they are a safety risk in enclosed spaces.
PLEASE NOTE

Every floor application is unique and needs a bespoke approach. This information is general technical guidance and does not replace a site assessment or the product’s MDS. Always confirm suitability with our certified professionals before specifying or installing.

Discuss your floor with our technical team