Skip to content
☎ +27 81 587 5010WhatsApp Find an ApplicatorSamples Data sheetsGallery
SUBSTRATES · 7 min read · Last reviewed: November 2026

How Do I Test for Moisture, and What if the Slab is Damp?

SHORT ANSWERGUIDE

Moisture is one of the most common causes of resin floor failure. Measure it with a recognised test, compare the result with the primer’s MDS limit, and where the slab is too damp, either wait, dry it, or use a moisture-tolerant primer system.

Why moisture matters

Moisture rising through a slab can build pressure beneath an impermeable resin layer, leading to blisters, loss of bond and, on epoxies, surface whitening. New slabs, ground-floor slabs without a damp-proof membrane and slabs in wet areas carry the highest risk.

Test methods compared

MethodWhat it tells youUse it for
In-situ hygrometer (sealed hood or drilled probe)Relative humidity in or on the slabThe reference method for acceptance
Calcium carbide (CM) testMoisture content of a drilled sampleConfirming readings, especially on screeds
Electronic surface meterComparative readings onlyFinding wetter areas, not for acceptance
Sealed plastic sheet testWhether moisture is risingA quick first check only

Decision flowchart

Is the reading within the primer’s MDS limit?Yes →Use the standard primer
Can the programme wait, or can the slab be dried?Yes →Dehumidify and ventilate, then retest
Is there rising damp with no damp-proof membrane?Yes →Seek technical advice before proceeding
Use a moisture-tolerant primer system within its MDS limits

Method overview

  1. Plan the test points. Include areas near external walls, doors, wet rooms and any visibly darker patches.
  2. Allow equilibrium time. Follow the time the test method requires before taking readings.
  3. Record conditions. Note air temperature and humidity with each reading.
  4. Compare with the MDS. Use the limit for the specific primer you intend to use.
  5. Decide and record. Standard primer, drying time, moisture-tolerant system, or further advice.

Common failure modes

SymptomLikely causePrevention
Blisters appearing weeks after installationMoisture rising from the slabTest before priming; moisture-tolerant system where needed
White bloom on an epoxy surfaceMoisture during cureControl conditions and substrate moisture
Debonding near walls and doorsLocalised dampTest at perimeters, not only mid-floor
Soft or poorly cured primerDamp surface at applicationUse a primer suited to the measured moisture
PLEASE NOTE

Every floor application is unique and needs a bespoke approach. This information is general technical guidance and does not replace a site assessment or the product’s MDS. Always confirm suitability with our certified professionals before specifying or installing.

Discuss your floor with our technical team