SHORT ANSWERGUIDE
Where different substrates meet, such as timber and concrete or a new extension against an old slab, they move, dry and absorb differently. Treat each side on its own terms and decide in advance how the junction will be detailed, usually with a movement joint.
Why junctions fail
A seamless floor makes two different substrates behave as one surface. Any difference in movement concentrates at the junction, and that is where cracks and debonding appear first.
What differs between substrates
- Movement: timber and new concrete move more than an old, stable slab.
- Moisture: a new slab can hold far more moisture than the old one next to it.
- Absorbency: old and new concrete take up primer at different rates, which can show as patchiness.
- Levels: extensions and repairs rarely meet the existing floor exactly.
- Contamination: old floors may carry oils, sealers or residues the new slab does not.
Old build compared with new build
| Factor | Old build | New build |
|---|---|---|
| Moisture | Usually dry, but still test | Often high. Test before any work |
| Surface | Contamination, previous coatings, wear | Laitance and curing compounds |
| Movement | Mostly stable | Drying shrinkage continues for months |
| Primer uptake | Can be high or uneven | Usually lower once laitance is removed |
| Levels | Settlement and dips | May sit high or low at the junction |
Detailing the junction
Identify and test each side separately
Is movement expected at the junction?Yes →Form or cut a movement joint and carry it through the new floor
Bond and fill the junction, reinforcing where the MDS allows
Level the junction
Prime each side to suit, then apply the system continuously
Method overview
- Survey both areas. Record substrate type, age and condition on each side.
- Test separately. Moisture and strength results from one side do not apply to the other.
- Let new work dry. New concrete and screeds must reach the MDS moisture limit.
- Prepare each side. Remove laitance on new work and contamination or coatings on old work.
- Level the junction. Correct steps and dips before priming.
- Detail the junction. Movement joint or bonded detail, decided in advance.
- Prime and apply. Adjust priming where absorbency differs.
- Trial area. Include the junction in the trial.
Common failure modes
| Symptom | Likely cause | Prevention |
|---|---|---|
| Straight crack at the junction | Differential movement | Movement joint at the junction |
| Blistering on the new side | New slab not dry enough | Moisture test before priming |
| Colour or gloss difference | Different absorbency | Prime to suit; extra primer coat on porous areas |
| Visible step or lip | Level difference | Level before coating |
PLEASE NOTE
Every floor application is unique and needs a bespoke approach. This information is general technical guidance and does not replace a site assessment or the product’s MDS. Always confirm suitability with our certified professionals before specifying or installing.